Bridge cracks repair methods

Once the crack appears, it will affect the structural durability, will directly affect the bearing capacity of the structure, and even endanger the safety of the structure. It is worthy of attention and should ascertain the cause of cracks,we must take appropriate measures to repair.

Bridge cracks repair methods


During the construction and operation of the bridge, there will be cracks, transverse, longitudinal and oblique cracks in different parts of the beam. Once the crack appears, it will affect the structural durability, will directly affect the bearing capacity of the structure, and even endanger the safety of the structure. It is worthy of attention and should ascertain the cause of cracks,we must take appropriate measures to repair.


1. The structure has little or no great influence on the structure itself, mainly by the way of surface sealing and repairing: mortar sealant, crack glue injection reinforcement, chisel inlay and surface shotcreting.


2. The structure has no effect, long-term erosion caused by rain and gas on the structure have a greater impact on the use of pressure grouting to repair, is a slurry (such as cement and epoxy resin grout) by applying certain pressure into the structure to achieve the internal crack, crack closure, restore and enhance the structure strength and durability and impermeability.


3. The larger cracks have damaged the structure. The following methods are dealt with: steel plate bonding reinforcement, carbon fiber fabric bonding and reinforcement, increasing beam section size reinforcement, prestressed carbon plate reinforcement and so on.

المنتجات الموصى بها

يمكنك العثور على أي شيء تحتاجه هنا ، ولديك ثقة في تجربة هذه المنتجات ، وسوف تجد الفرق الكبير بعد ذلك.

ألياف الكربون أحادية الإتجاة

تستخدم المواد البولیمریة المسلحة بألیاف الکربون في العدید من تطبیقات الهندسة الإنشائیة کتدعیم الأعمده، الکمرات، الجدران، البلاطات و الأسقف في المنشآت و المباني

أكثر من >

شرائح الکربون

شرائح FRP المنضدة هی عبارة عن شرائح تبلغ سماکتها میلی متر او اکثر و تتمتع بمقاومة عالیة فی اتجاة واحد او اثنین و یتم تلصیقها علی الخرسانة او الصلب باستخدام راتنجات FRP ایبوکسیة خاصة.

أكثر من >

ايبوكسي حقن الشقوق

یعبر عن حقن راتنجات الایبوکسي الرقیقة العاریة من المذیبات بحقن الراتنجات. لتطبیق هذا المنتج یجب تعبیة صوامیل الحقن في العنصر المطلوب و من ثم حقن الراتنج بشکل یدوي أو میکانیکي من خلال هذة الصوامیل. یستعمل حقن الراتنج بشکل واسع في معالجة العناصر الکونکریتة م

أكثر من >